Peel Strength 0.11504 kN/m
0.65625 pli
to Steel; ASTM D3330
3M Scotch® 4737S High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..
Peel Strength 0.11504 kN/m
0.65625 pli
to Steel; ASTM D3330
3M Scotch® 4737T High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..