Polymer Property : Peel Strength = 1.030 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
3M 9828PC Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
3M 9832 Double Coated Tapes with Adhesive 300MP
3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7903FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7905 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7909 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
3M 9828HL Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Peel Strength 1.030 kN/m
5.875 pli
90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
3M 7997MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
3M 9828 Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Peel Strength 1.030 kN/m
5.875 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
3M 9832HL Double Coated Tapes with Adhesive 300MP
3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape..