Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 100 kN/m | >= 571 pli | 90+5°C; ISO 21809-1 |
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&.. |