Peel Strength >= 100 kN/m
>= 571 pli
90+5°C; ISO 21809-1
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating
Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&..