Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | Ply-Adhesion; Arlon SQA-TMS-011 |
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | Bond Strength; ASTM D624 |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | Bond Strength; ASTM D624 |
Arlon 55900R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Appearance: Red silicone gum on glass fabricThis data represents typical values for the p.. |
|||
Peel Strength | 2.10 kN/m @Temperature 60.0 °C, Time 605000 sec |
12.0 pli @Temperature 140 °F, Time 168 hour |
JRF, Alcad; STM 40-107 |
3M AC-645 B-2 Aerospace Sealant 3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli.. |
|||
Peel Strength | 2.10 kN/m @Temperature 60.0 °C, Time 6.05e+6 sec |
12.0 pli @Temperature 140 °F, Time 1680 hour |
JRF, Alcad; STM 40-107 |
3M AC-645 B-2 Aerospace Sealant 3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | |
Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | |
Arlon AD450A Glass, PTFE and Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD600 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Ceramic Filled High Dielectric ConstantMechanically Robust; replaces brittle laminates that cannot withstand processing, impact or High G forcesLarge Panel SizesHigh Peel Strength for Narrow LinesBe.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | T-Peel, Initial |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to Copper, Mastic; ASTM D1000 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to PVC, Mastic; ASTM D1000 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to Polyethylene, Mastic; ASTM D1000 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to Copper, Mastic; ASTM D1000 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to PVC, Mastic; ASTM D1000 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to Polyethylene, Mastic; ASTM D1000 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to EPR, Mastic; ASTM D1000 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to PVC, Mastic; ASTM D1000 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to Polyethylene, Mastic; ASTM D1000 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | Adhesion to EPR, Mastic; ASTM D1000 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Peel Strength | >= 2.10 kN/m | >= 12.0 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | 180°, Scott Tensile Tester |
3M Scotch-Weld™ 4550 Industrial Adhesive Features: It is a sprayable, synthetic elastomer based adhesive for bonding many lightweight materials such as felt, cork, cardboard, and paper to metal and other substratesIdeal for palletizing “a.. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | Aluminum-Supported Vinyl, 180°, Aging 7 Day @ 100% RH |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | on canvas |
3M Scotch-Weld™ 3750 Clear Hot Melt Adhesive Low viscosity for high flow rate, increased production and Good hot tack, quick grab for packaging and woodworkingInformation provided by 3M |
|||
Peel Strength | 2.10 kN/m | 12.0 pli | T-Peel, Initial |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |