Polymer Property : Peel Strength = 2.40 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.421 kN/m
2.40 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
3M 7214SA Screen Printable Polyester Performance Label Products with Structured Adhesive
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc..
Peel Strength 0.421 kN/m
2.40 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
3M 7215SA Screen Printable Polyester Performance Label Products with Structured Adhesive
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc..
Peel Strength 0.421 kN/m
2.40 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
3M 7218SA Screen Printable Polyester Performance Label Products with Structured Adhesive
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc..
Peel Strength 0.421 kN/m
2.40 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
3M 7220SA Screen Printable Polyester Performance Label Products with Structured Adhesive
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc..
Peel Strength 0.421 kN/m
2.40 pli
Bond Strength; Arlon SQA-TMS-015
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec..