3M 7220SA Screen Printable Polyester Performance Label Products with Structured Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7220SA Screen Printable Polyester Performance Label Products with Structured Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label stocks utilize 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metals. With unique microchannels throughout the structured adhesive, air flows freely from between the adhesive and substrate. Hand applied labels go on smoothly and stay that way. Even when labels are used on injection-molded plastic parts, bubbles that form from plastic outgassing can be smoothed to regain a neat appearance for the graphic.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
50.8 microns
2.00 mil
Facestock
198 microns
7.80 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.421 kN/m
2.40 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.543 kN/m
3.10 pli
Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.543 kN/m
3.10 pli
Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.666 kN/m
3.80 pli
Stainless Steel, 180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type 350
Liner 90# Embossed Polycoated