Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.60259 kN/m | 3.4375 pli | Adhesion, silicone side |
Dielectric Polymers NT-1020 Silicone/Acrylic Double Coated Tape
(discontinued **) Crosslinked silicone and acrylic adhesive with 2 mil polyester film release liner backing on the silicone side and moisture stable PE coated kraft (60#) on the acrylic side.Features: Chemical resist.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9505 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9672 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Urethane-B, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Urethane-B, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1060 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1060 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1920S Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1040 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1040 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | to Steel |
3M 3939 Duct Tape 3M™ Duct Tape 3939 is composed of waterproof polyethylene film over cloth scrim backing with a rubber adhesive used for demanding duct tape applications.Information provided by 3M |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Adhesion to Steel; ASTM D3330 |
3M 5453 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5453 has a silicone adhesive which provides a high temperature release surface for protection and insulation.Information provided by 3M |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1015M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1020M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 3785 Performance Continuous Taping System Tape Scotch® Performance Continuous Taping System Tapes 3785 is a packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. These tapes.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.60259 kN/m | 3.4375 pli | ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9555 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |