Mechanical Properties Metric English Comments
Peel Strength 0.771 kN/m

@Temperature 121 °C,
Time 605000 sec
4.40 pli

@Temperature 250 °F,
Time 168 hour
ASTM D1000
Parker Chomerics CHO-FOIL CCD Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Peel Strength 0.771 kN/m
4.40 pli
Bond Strength; Arlon SAQ-TMS-011
Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ..
Peel Strength 0.771 kN/m
4.40 pli
Adhesion to Aluminum, anodized
3M Controltac™ 160 Graphic Film
4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha..
Peel Strength 0.771 kN/m
4.40 pli
Cold Rolled Steel, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Peel Strength 0.771 kN/m
4.40 pli
PP 90° Peel, 72 hr dwell, 300 mm/min
3M 9343 Conformable Sound Management Film
3M™ Conformable Sound Management Film 9343 is designed for the reduction of noise, vibration, squeaks, and rattles in automotive interior applications. The currently available materials for these a..
Peel Strength 0.771 kN/m
4.40 pli
Initial; ASTM D1000
Parker Chomerics CHO-FOIL CAD Shielding Tape
Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ..