Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.894 kN/m | 5.10 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Peel Strength | 0.894 kN/m | 5.10 pli | (S1 to S2) Bond Strength; Arlon SQA-TMS-011 |
Arlon 48271R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater .. |
|||
Peel Strength | 0.894 kN/m | 5.10 pli | Bond Strength (S1 to S1); ASTM D624 |
Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typic.. |