Polymer Property : Peel Strength = 58.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 10.2 kN/m

@Temperature 21.1 °C
58.0 pli

@Temperature 70.0 °F
Bell Peel
Hexcel® Redux® 308A-NA Modified epoxy film adhesive
Redux 308A-NA is a high-strength, flow-controlled film adhesive with flexible cure schedules at 300°F or 350°F. Redux 308A-NA contains glass beads that give good flow control. It is suitable for m..