Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.877 - 1.23 kN/m | 5.00 - 7.00 pli | |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Peel Strength | 0.877 - 1.23 kN/m | 5.00 - 7.00 pli | |
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
Peel Strength | 0.877 - 1.23 kN/m | 5.00 - 7.00 pli | Adhesion to Aluminum, anodized |
3M Envision™ 480Cv3 Print Wrap Film High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubb.. |