Material Notes:
Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It has a medium paste like viscosity, which gives minimal sag upon cure at elevated temperature. Being a 100% solids, single component product a variety of simple, low cost dispensing methods are available for application of this product. This product will cure at temperatures as low as 113°C (235°F) without sacrificing shelf life or need for unusual shipping or storage considerations.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
TM R050-16
Water Absorption 2.08 %

@Time 86400 sec
2.08 %

@Time 24.0 hour
TM R050-35
Viscosity 750000 cP
750000 cP
RVT, #7, 2.5 rpm; TM R050-12
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
TM R050-17
Tensile Strength at Break 37.9 MPa
5500 psi
TM R050-36
Tensile Strength, Ultimate 37.9 MPa
5500 psi
TM R050-36
Tensile Strength, Yield 17.2 MPa
2500 psi
TM R050-36
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
TM R050-36
Tensile Modulus 4.14 GPa
600 ksi
TM R050-36
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Peel Strength 0.877 - 1.23 kN/m
5.00 - 7.00 pli
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 123 °C
253 °F
TM R050-25
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+12 ohm-cm
8.00e+12 ohm-cm
Dielectric Constant 4.5

@Frequency 100 Hz,
Temperature 25.0 °C
4.5

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 16.1 kV/mm
410 kV/in
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 177 °C
0.333 hour

@Temperature 351 °F
40.0 min

@Temperature 150 °C
0.667 hour

@Temperature 302 °F
45.0 min

@Temperature 135 °C
0.750 hour

@Temperature 275 °F
150 min

@Temperature 121 °C
2.50 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Color Gray
Pot Life (Months) 3
at 25°C, Mass: 100g
6
at <10°C, Mass: 100g