Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.2600 kN/m | 7.1875 pli | to stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 444 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | to stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 444PC Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9472LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9579 Double Coated Tape with Adhesive 760 3M™ Double Coated Tape 9579 with 3M™ Adhesive 760 is a high-tack, hand-tearable, double coated film tape with a pressure sensitive adhesive on each side of the carrier. The medium firm adhesive fe.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | 72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.2600 kN/m | 7.1875 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |