Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.3695 kN/m | 7.8125 pli | 72 hr, Linered side-PVC; ASTM D3330 |
3M 2205 Thin Flexographic Plate Mounting Tape 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business .. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | Stainless Steel, Ultimate Bond, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330 |
3M 9437 Adhesive Transfer Tape with Adhesive 100MP 3M™ Adhesive Transfer Tape 9437 with 3M™ Adhesive 100MP is designed for harsh environments such as automotive, aerospace and outdoor applications.Features:Excellent temperature and chemical resist.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | Acrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | Acrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9675 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | 90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | ABS, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | Acrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9445 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.3695 kN/m | 7.8125 pli | Acrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485EK Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |