Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.40 kN/m | 8.00 pli | 1 oz. Cu, after exposure to process solutions; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | 180°, Teak (primed), 50% RH |
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | 90° Angle Peel 12 in./min. Jaw Speed (308 mm/min.) 72 hour Dwell; ASTM D3330 |
3M 4462B Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ 1000-13 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ 1000-77 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-11 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-114 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-196 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-197 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-20 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-37 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-46 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-63 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-187 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-25 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-63 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ FN3650-114 Graphic Film 2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M |
|||
Peel Strength | >= 1.40 kN/m | >= 8.00 pli | [ppi], Bond Strength |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Bond Strength; Arlon-SQA-TMS-011 |
Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ 1000-196 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ 1000-38 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-14 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-22 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7125-98 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-48 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | Adhesion to Aluminum, alodine |
3M Scotchcal™ ElectroCut™ 7725-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | >= 1.40 kN/m | >= 8.00 pli | Bond Strength |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
Peel Strength | 1.40 kN/m | 8.00 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi.. |