Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.0%); ASTM-D638
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature 80.0 °C
17400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature 80.0 °C
17400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 120 MPa

@Temperature 80.0 °C
17400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..