Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 190 - 210 MPa @Temperature 23.0 - 1500 °C |
27600 - 30500 psi @Temperature 73.4 - 2730 °F |
|
UBE Tyrannohex® Heat Resistant Composite Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe.. |