Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 720 MPa @Thickness 1.10 - 1.60 mm, Temperature 649 °C |
104000 psi @Thickness 0.0433 - 0.0630 in, Temperature 1200 °F |
|
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Ultimate | 720 MPa @Temperature 550 °C |
104000 psi @Temperature 1020 °F |
Precipitation Hardened prior to test |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |