Polymer Property : Tensile Strength, Ultimate = 785 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 785 MPa

@Temperature 600.0 °C
114000 psi

@Temperature 1112 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..
Tensile Strength, Ultimate 785 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
114000 psi

@Thickness 0.500 in,
Temperature 77.0 °F
as welded
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..