Mechanical Properties Metric English Comments
Tensile Modulus 0.550 GPa

@Temperature 23.0 °C
79.8 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Tensile Modulus 0.550 GPa

@Temperature 120 °C
79.8 ksi

@Temperature 248 °F
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Tensile Modulus 0.550 GPa

@Temperature 60.0 °C
79.8 ksi

@Temperature 140 °F
LATI Latamid 6 BH PA 6, Heat Stabilized
Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
Tensile Modulus 0.550 GPa

@Temperature 90.0 °C
79.8 ksi

@Temperature 194 °F
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..
Tensile Modulus 0.550 GPa

@Temperature 90.0 °C
79.8 ksi

@Temperature 194 °F
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Tensile Modulus 0.550 GPa

@Temperature 60.0 °C
79.8 ksi

@Temperature 140 °F
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N..