Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 10.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.2 GPa

@Temperature 23.0 °C
1480 ksi

@Temperature 73.4 °F
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 10.2 GPa

@Temperature 23.0 °C
1480 ksi

@Temperature 73.4 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..