Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.7 GPa @Temperature 60.0 °C |
1990 ksi @Temperature 140 °F |
|
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Modulus | 13.7 GPa @Temperature 90.0 °C |
1990 ksi @Temperature 194 °F |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |