Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.80 GPa @Temperature 23.0 °C |
1420 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.80 GPa @Temperature 23.0 °C |
1420 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.80 GPa @Temperature 120 °C |
1420 ksi @Temperature 248 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 9.80 GPa @Temperature 23.0 °C |
1420 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 9.80 GPa @Temperature 60.0 °C |
1420 ksi @Temperature 140 °F |
|
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 9.79 GPa @Temperature 177 °C |
1420 ksi @Temperature 351 °F |
[+/-45°]; Resin Content=27%, Fiber Volume=66%; Wet condition-96 hours in boiling H2O |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |