Polymer Property : Tensile Modulus = 15790 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 108.9 GPa

@Temperature 71.0 °C
15790 ksi

@Temperature 160 °F
1/2 hr
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape
STD MOD FiberInformation provided by HexCel