Mechanical Properties Metric English Comments
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Tensile Modulus 2.40 GPa

@Temperature 150 °C
348 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Modulus 2.40 GPa

@Temperature 150 °C
348 ksi

@Temperature 302 °F
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 2.40 GPa

@Temperature 120 °C
348 ksi

@Temperature 248 °F
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
Tensile Modulus 2.40 GPa

@Temperature 150 °C
348 ksi

@Temperature 302 °F
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;..
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
LATI Latamid SP1 PA 6.10
Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
LATI Latilon 28D PC
Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
LATI Later 4 PBT
Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..