Mechanical Properties Metric English Comments
Tensile Modulus 15.0 GPa

@Temperature 90.0 °C
2180 ksi

@Temperature 194 °F
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 15.0 GPa

@Temperature 150 °C
2180 ksi

@Temperature 302 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Modulus 15.0 GPa

@Temperature 90.0 °C
2180 ksi

@Temperature 194 °F
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 15.0 GPa

@Temperature 120 °C
2180 ksi

@Temperature 248 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 15.0 GPa

@Temperature 23.0 °C
2180 ksi

@Temperature 73.4 °F
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 15.0 GPa

@Temperature 120 °C
2180 ksi

@Temperature 248 °F
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 15.0 GPa

@Temperature 23.0 °C
2180 ksi

@Temperature 73.4 °F
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 15.0 GPa

@Temperature 23.0 °C
2180 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers