Tensile Modulus 1.57 GPa

@Temperature 149 °C
228 ksi

@Temperature 300 °F
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e..