Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 261 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Tensile Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Tensile Modulus 1.80 GPa

@Temperature 60.0 °C
261 ksi

@Temperature 140 °F
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
Tensile Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i..
Tensile Modulus 1.80 GPa

@Temperature 150 °C
261 ksi

@Temperature 302 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 1.80 GPa

@Temperature 90.0 °C
261 ksi

@Temperature 194 °F
LATI Latilon 28D PC
Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 1.80 GPa

@Temperature 90.0 °C
261 ksi

@Temperature 194 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66  (Unverified Data**)
Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved