Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Zytel® FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont |
|||
Tensile Modulus | 3.40 GPa @Temperature 120 °C |
493 ksi @Temperature 248 °F |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 150 °C |
493 ksi @Temperature 302 °F |
|
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
|
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 60.0 °C |
493 ksi @Temperature 140 °F |
|
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 90.0 °C |
493 ksi @Temperature 194 °F |
|
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 150 °C |
493 ksi @Temperature 302 °F |
|
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 60.0 °C |
493 ksi @Temperature 140 °F |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
|
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 90.0 °C |
493 ksi @Temperature 194 °F |
|
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |