Mechanical Properties Metric English Comments
Tensile Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66  (Unverified Data**)
Zytel® FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont
Tensile Modulus 3.40 GPa

@Temperature 120 °C
493 ksi

@Temperature 248 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.40 GPa

@Temperature 150 °C
493 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Tensile Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Tensile Modulus 3.40 GPa

@Temperature 60.0 °C
493 ksi

@Temperature 140 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 3.40 GPa

@Temperature 90.0 °C
493 ksi

@Temperature 194 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Modulus 3.40 GPa

@Temperature 150 °C
493 ksi

@Temperature 302 °F
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 3.40 GPa

@Temperature 60.0 °C
493 ksi

@Temperature 140 °F
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
Tensile Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea..
Tensile Modulus 3.40 GPa

@Temperature 90.0 °C
493 ksi

@Temperature 194 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..