Polymer Property : Tensile Modulus = 3.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Tensile Modulus 3.80 GPa

@Temperature 120 °C
551 ksi

@Temperature 248 °F
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 3.80 GPa

@Temperature 120 °C
551 ksi

@Temperature 248 °F
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Tensile Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
Tensile Modulus 3.80 GPa

@Temperature 120 °C
551 ksi

@Temperature 248 °F
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Improved thermal stabilization. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In..
Tensile Modulus 3.80 GPa

@Temperature 120 °C
551 ksi

@Temperature 248 °F
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 3.80 GPa

@Temperature 150 °C
551 ksi

@Temperature 302 °F
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri..
Tensile Modulus 3.80 GPa

@Temperature 120 °C
551 ksi

@Temperature 248 °F
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66  (Unverified Data**)
Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers
Tensile Modulus 3.80 GPa

@Temperature 90.0 °C
551 ksi

@Temperature 194 °F
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La..