Polymer Property : Tensile Modulus = 3050 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.0 GPa

@Temperature 23.0 °C
3050 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 21.0 GPa

@Temperature 90.0 °C
3050 ksi

@Temperature 194 °F
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 21.0 GPa

@Temperature 23.0 °C
3050 ksi

@Temperature 73.4 °F
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 21.0 GPa

@Temperature 24.0 °C
3050 ksi

@Temperature 75.2 °F
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F161; Fiber: 450-1/2Information provided by HexCel
Tensile Modulus >= 21.0 GPa

@Temperature 100 °C
>= 3050 ksi

@Temperature 212 °F
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..