Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 25.0 GPa @Temperature 23.0 °C |
3630 ksi @Temperature 73.4 °F |
|
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 25.0 GPa @Temperature 23.0 °C |
3630 ksi @Temperature 73.4 °F |
|
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Modulus | 25.0 GPa @Temperature 71.0 °C |
3630 ksi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric Fiber: Kev. 49 195Information provided by HexCel |