Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 53.8 GPa @Temperature 71.0 °C |
7800 ksi @Temperature 160 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel |
|||
Tensile Modulus | 53.8 GPa @Temperature 93.0 °C |
7800 ksi @Temperature 199 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |