Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 6.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.30 GPa

@Temperature 60.0 °C
914 ksi

@Temperature 140 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 6.30 GPa

@Temperature 90.0 °C
914 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 6.30 GPa

@Temperature 150 °C
914 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 6.30 GPa

@Temperature 90.0 °C
914 ksi

@Temperature 194 °F
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 6.30 GPa

@Temperature 23.0 °C
914 ksi

@Temperature 73.4 °F
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 6.30 GPa

@Temperature 60.0 °C
914 ksi

@Temperature 140 °F
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 6.30 GPa

@Temperature 23.0 °C
914 ksi

@Temperature 73.4 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 6.30 GPa

@Temperature 23.0 °C
914 ksi

@Temperature 73.4 °F
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North..
Copyright © lookpolymers.com All Rights Reserved