Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.30 GPa @Temperature 120 °C |
1060 ksi @Temperature 248 °F |
|
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Tensile Modulus | 7.30 GPa @Temperature 60.0 °C |
1060 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 7.30 GPa @Temperature 60.0 °C |
1060 ksi @Temperature 140 °F |
|
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La.. |