Mechanical Properties Metric English Comments
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 9.00 GPa

@Temperature 90.0 °C
1310 ksi

@Temperature 194 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Tensile Modulus 9.00 GPa

@Temperature 150 °C
1310 ksi

@Temperature 302 °F
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &..
Tensile Modulus 9.00 GPa

@Temperature 120 °C
1310 ksi

@Temperature 248 °F
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66
Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66  (Unverified Data**)
Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im..
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 9.00 GPa

@Temperature 120 °C
1310 ksi

@Temperature 248 °F
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
Zytel® 70G35HSRX BK099 a 35% glass reinforced, heat stabilized, hydrolysis resistant PA66 for injection molding. Developed for applications designed for direct overmolding of gaskets onto thermopla..