Mechanical Properties Metric English Comments
Tensile Modulus 9.20 GPa

@Temperature 23.0 °C
1330 ksi

@Temperature 73.4 °F
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa..
Tensile Modulus 9.20 GPa

@Temperature 60.0 °C
1330 ksi

@Temperature 140 °F
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 9.20 GPa

@Temperature 120 °C
1330 ksi

@Temperature 248 °F
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 9.20 GPa

@Temperature 120 °C
1330 ksi

@Temperature 248 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Modulus 9.20 GPa

@Temperature 23.0 °C
1330 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Tensile Modulus 9.20 GPa

@Temperature 23.0 °C
1330 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel
Tensile Modulus 9.20 GPa

@Temperature 90.0 °C
1330 ksi

@Temperature 194 °F
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..