Polymer Property : Compressive Strength = 0.0700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0700 - 0.110 MPa

@Strain 40.0 %
10.2 - 16.0 psi

@Strain 40.0 %
BS4443 Part 1 Method 5B
P & P Technology Silicone Sponge
The thermal stability of silicone rubber is probably its most important asset. Components made from these rubbers are affected only to a small extent by extremes of temperature, ranging from –90°C..
Compressive Strength 0.0700 MPa

@Strain 10.0 %
10.2 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Compressive Strength 0.0700 MPa

@Strain 10.0 %
10.2 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..