Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

P & P Technology Silicone Sponge

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology Silicone Sponge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The thermal stability of silicone rubber is probably its most important asset. Components made from these rubbers are affected only to a small extent by extremes of temperature, ranging from –90°C to 250°C (depending on grade). Even at temperatures as high as 300°C Silicone rubber will operate for limited periods. Silicone rubber is an excellent electrical insulating material. Resistance to arcing corona, ultra-violet light and ozone is good. It decomposes at 400°C to 500°C leaving an inert, non-flammable and electrically non-conductive residue. It is made of a fine cellular construction composed mainly of non-interconnecting cells and are normally of an off-white color. For continuous use it will stand temperatures between –60°C and -200°CInformation provided by P & P Technology
Mechanical Properties Metric English Comments
Compressive Strength 0.0700 - 0.110 MPa

@Strain 40.0 %
10.2 - 16.0 psi

@Strain 40.0 %
BS4443 Part 1 Method 5B
0.900 MPa

@Strain 40.0 %
131 psi

@Strain 40.0 %
BS4443 Part 1 Method 5B
Compression Set 5.0 %

@Temperature 150 °C,
Time 252000 sec
5.0 %

@Temperature 302 °F,
Time 70.0 hour
recovery period 48 hours 25% compression, after 168 hours at 150°C; BS4443 Part 1 Method 6A
6.0 %

@Temperature 150 °C,
Time 252000 sec
6.0 %

@Temperature 302 °F,
Time 70.0 hour
recovery period 48 hours 25% compression,; BS4443 Part 1 Method 6A
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Continuous use
250 °C
482 °F
Components made from product
300 °C
572 °F
Limited periods
Minimum Service Temperature, Air -90.0 °C
-130 °F
Components made from product
-60.0 °C
-76.0 °F
Continuous use
Users viewing this material also viewed the following: