Compressive Strength 103 MPa

@Temperature 110 °C
14900 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC95 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 103 MPa

@Strain 2 %
14900 psi

@Strain 2 %
ISO 604
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data)
This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural..