Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 103 MPa @Temperature 110 °C |
14900 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 103 MPa @Strain 2 % |
14900 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |