Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 112 MPa @Strain 5 % |
16200 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |