Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 118 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 118 MPa

@Strain 2 %
17100 psi

@Strain 2 %
ISO 604
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..
Compressive Strength 118 MPa

@Temperature 1500 °C
17100 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics REFCAST ULCC90 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 118 MPa

@Temperature 1500 °C
17100 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 003 Smart Cast Application
Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 118 MPa

@Temperature 1500 °C
17100 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 004 Smart Cast Application
Special Properties: Thermal Shock, Abrasion, Alkali ResistanceIndustry: SteelApplication: Lances, Launders, Riser TubesInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 118 MPa

@Temperature 1100 °C
17100 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 007 Smart Cast Application
Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 118 MPa

@Temperature 1100 °C
17100 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC95 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 118 MPa

@Temperature 1500 °C
17100 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 011 Smart Cast Application
Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 118 MPa

@Temperature 1500 °C,
Time 10800 sec
17100 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 118 MPa

@Temperature 1400 °C,
Time 10800 sec
17100 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-60KL Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 118 MPa

@Temperature 1350 °C,
Time 10800 sec
17100 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-70 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved