Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.80 g/cc
>= 0.101 lb/in³
After Drying at 110°C
Grain Size <= 10000 µm
<= 10000 µm
Mechanical Properties Metric English Comments
Compressive Strength 78.5 MPa

@Temperature 110 °C
11400 psi

@Temperature 230 °F
Cold Crushing
98.1 MPa

@Temperature 1100 °C
14200 psi

@Temperature 2010 °F
Cold Crushing
118 MPa

@Temperature 1500 °C
17100 psi

@Temperature 2730 °F
Cold Crushing
29.4 MPa

@Time 86400 sec
4270 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1600 °C
2910 °F
Descriptive Properties Value Comments
Refractoriness >1720°C
Thermal Expansion 0.9
Reversible
Water Required to Mix 9-11%