Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.76 MPa @Treatment Temp. 104 °C |
400 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2300 Insulating Castable Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f.. |
|||
Compressive Strength | 2.76 MPa @Treatment Temp. 104 °C |
400 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2100 Insulating Castable Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn.. |