Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |