Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 15.0 MPa @Strain 2 % |
2180 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Compressive Strength | 15.0 MPa @Strain 2 % |
2180 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Compressive Strength | 15.0 - 25.0 MPa @Temperature 1000 °C |
2180 - 3630 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |
|||
Compressive Strength | 15.0 - 21.0 MPa @Temperature 100 °C |
2180 - 3050 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |