Mechanical Properties Metric English Comments
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
Result based on 450GL30; ISO 604
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Compressive Strength 160 MPa

@Temperature 120 °C
23200 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..